Laminated Category

Laminated wood is made by bonding multiple layers of timber with strong adhesives under heat and pressure, enhancing strength and stability. This engineered structure minimizes warping and cracking over time. It is Ideal for both structural and decorative applications across construction and interior design.

  • Structure: hydrothermal modification according to the ISO 13061-2:2014 standard 
  • Color: Can be customized upon request 
  • Category: Poplar, Ash, Pine, Oak 
  • Our dimensions (or customize your own)(inch): 

Length:  48 -192

Width: 4 - 8

Thickness: ⅜ - ½ 

  • Surface Hardness: 1,32 (N/mm2) according to % EN 13329:2016 standard 
  • Expansion rate or water absorption: 1,84%
  • Formaldehyde emission = E1/E0
  • Finish:  2K or UV coating 
  • Moisture content: 10+-2% according to TCVN 13707-1:2023 (Equivalent to ISO 13061-1:2014 with Amendment 1:2017)
  • Termite Resistance: Rated Level 3 according to TCVN 11355:2016.
  • Mold and Stain Fungus Resistance: Rated Level 3 according to TCVN 11356:2016.
  • Features: Minimizes warping, shrinkage, cracking, and termite damage. Reduces swelling, prevents brittleness and chipped edges. Improves static bending strength (MOR) and parallel grain strength, while enhancing color stability.
  • Applications: flooring, interior furniture